← All published pairs
Acrylic adhesive on LDPE
2 verified lap-shear rows from manufacturer datasheets. Values stay with the surface preparation printed on the sheet.
| Product | Prep | Strength | Standard | Source |
|---|---|---|---|---|
| 3M Scotch-Weld Structural Plastic Adhesive DP8010 Overlap Shear Strength. Temperature: 23 °C (73 °F). Dwell Time: 7 d. Test Method: ASTM D1002, ISO 4587. Low Density Polyethylene (LDPE) IPA Wipe 360 lb/in². (SF). | degreased | 2.4821 MPa | ASTM D1002, ISO 4587 | TDS p.2 |
| 3M Scotch-Weld Structural Plastic Adhesive DP8010NS Blue Overlap Shear (psi), ASTM D1002. DP8010NS Blue column: LDPE (IPA wipe) 360. Cured 7 days at room temperature. | degreased | 2.4821 MPa | ASTM D1002 | TDS p.3 |