← All published pairs

Methyl cyanoacrylate on Steel

3 verified lap-shear rows from manufacturer datasheets. Values stay with the surface preparation printed on the sheet.

ProductPrepStrengthStandardSource
LOCTITE 415

Steel (grit blasted) N/mm² 20 to 30 (psi) (2,900 to 4,350)

grit blasted20–30 MPaISO 4587TDS p.2
LOCTITE 430

Steel (grit blasted) N/mm² 20 to 30 (psi) (2,900 to 4,350)

grit blasted20–30 MPaISO 4587TDS p.2
LOCTITE 493

Steel (grit blasted) N/mm² 20 to 30 (psi) (2,900 to 4,350)

grit blasted20–30 MPaISO 4587TDS p.2

Steel material page